IDT-Grooved Gasket WS 1.4571-3803-KD10-20-30-5.0 mm - Printable Version +- European Sealing Association (https://forum.bacibg.org) +-- Forum: Flange Gaskets (https://forum.bacibg.org/forumdisplay.php?fid=1) +--- Forum: Gasket Database (https://forum.bacibg.org/forumdisplay.php?fid=2) +---- Forum: ESAData Approved Datasheets (https://forum.bacibg.org/forumdisplay.php?fid=10) +---- Thread: IDT-Grooved Gasket WS 1.4571-3803-KD10-20-30-5.0 mm (/showthread.php?tid=194) |
IDT-Grooved Gasket WS 1.4571-3803-KD10-20-30-5.0 mm - AMTEC - 12-13-2022 We recognized a mistake in the input data for creating the datasheet of the material IDT-Grooved Gasket with graphite layer-WS 1.4571-3803-KD10-20-30-5.0 mm In the data of the leakage tests at 10 and 40 bar in the unoading curve starting at 60 MPa there was a gasket stress level indicated with 40 MPa instead of 20 MPa. This mistake influences the characteristics QSmin(L) slightly. In the attached draft of the revised datasheet the characteristics which will change are highlighted yellow. RE: IDT-Grooved Gasket WS 1.4571-3803-KD10-20-30-5.0 mm - Garlock - 12-13-2022 Note1: Compared to 10bar, 40bar and 80bar Leak rates curves of 160bar (on last page) indicate that (longer?) holding time for mass spectrometere is accurate, but the scale looks differrent than expected. All other graphs always do end up with 1,0 x 10 E-02 but the 160bar does end up within 1,0x10E-01 sector if less than 31MPa is given. Note2: Where can i find these 31MPa in table "Minimum required gasket stress in service (QSmin/L) --> Here, <20MPa is given instead of 31MPa |